Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

Categories Cobalt Alloy Castings
Brand Name: Eternal Bliss
Model Number: EB26078
Certification: ISO9001-2008
Place of Origin: China
MOQ: 30 kg
Price: USD80/kg ~ USD120/kg
Payment Terms: by T/T or L/C, Western Union
Supply Ability: 100,000,000.00
Delivery Time: It depends on the quantity to be ordered.
Packaging Details: Pallets
Material Grade: cobalt alloy 1, cobalt alloy 3,
Hardness Temperature: Up to 1200 Centi-degree
Coating Process: SPF Coating,overlay process
Cast Process: Wax Lost Process
Surface Treatment: Shot Blast
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

Precision Cast Process X-40 Cobalt High Speed Steel Products with High Accuracy EB26078

.


Precision investment casting services for a variety of high temperature super alloys cobalt-based types.

Provides on-site engineering support, tooling design, surface treatment, laboratory testing, and warehousing services. Just in time delivery and other logistics services are available.


We produce High Temperature Superalloy Castings Parts with precision investment process.


Table 1 : Standard Cobalt cobalt alloy Alloy

CoCrCWMoNiSiBFeMnOthers
cobalt alloy 1BAL332.4513-2.5*1-2.5*1-
cobalt alloy 3BAL312.513-2.5*1-2.5*1-
cobalt alloy 4BAL31.5114-2.0*1-2.0*1-
BAL281.25-3.0*1-2.5*1-
cobalt alloy 12BAL291.859-2.5*1-2.5*1-
cobalt alloy 20BAL332.4517.5-2.5*1-2.5*1-
cobalt alloy 21BAL270.25-5.52.5*1-3.0*1-
cobalt alloy 31BAL260.57.5-10.51-2.0*1-
cobalt alloy 190BAL263.314-1.01-8.00.5-
cobalt alloy 238BAL260.1-3-1-20.01-
cobalt alloy 306BAL250.42-6.01-4.0*1Nb=5
94BAL28119-5.01-2.5*1V=1
cobalt alloy FBAL25.51.7512.25-22.51-1.5*--
cobalt alloy SF1BAL191.313-1332.53*0.5Cu=0.5
cobalt alloy SF6BAL190.77-132.51.73*0.5Cu=0.5
cobalt alloy SF12BAL1919-13323*0.5Cu=0.5
cobalt alloy SF20BAL191.515-13332*0.5Cu=0.5
TRIBALOY T400BAL80.1*-283*2.4-3*--
TRIBALOY T800BAL170.1*-283*3.2-3*--
DELORO 15--0.06*--BAL2.01.051.5*20Cu=20
DELORO 22-0.700.10--BAL2.31.75---
DELORO 40-7.00.10--BAL3.52.25---
DELORO 50-10.250.45--BAL4.01.854.0--
DELORO 60-14.250.6--BAL2.03.54.0--
DELORO 625-220.1-9BAL--5--
NISTELLE C-16.50.12*4.517BAL0.7-6.0--
TRIBALOY T700-150.10*-32BAL3.25-
Hastelloy C22®(UNS N06022)(Max.)
CMNPSSiCrNiMoCOFeWV
0.0150.50.020.020.0820.0-22.5Bal.12.5-14.52.52.0-6.02.5-3.50.35
Hastelloy C276®(UNS N10276)(Max.)
CMNPSSiCrNiMoCOFeWV
0.0110.040.030.0814.5-16.5Bal.15.0-17.02.54.0-7.03.0-4.50.35
Hastelloyx®(UNS N06002)(Max.)
CMNPSSiCrNiMoCOFeWother
0.05-0.1510.040.03120.5-23.0Bal.8.0-10.00.5-2.517.0-20.00.2-1.0/
Monel 400®(UNS NO4400) (Max.)
CMNSSiNiCuFe
0.320.0240.563 min28-342.5
Monel M400®(UNS NO4400)(Max.)
CMNSSiNiCuFe
0.320.0240.563-7028-342.5
Monel R405®(UNS NO4405)(Max.)
CMNSSiNiCuFe
0.320.025-0.060.563.0min28-342.5
Monel K500®(UNS NO5500)(Max.)
CMNSSiNiCuTiAIFe
0.120.010.563min27-330.862.3-3.152
Inconel 600(UNS NO6600)(Max.)
CMNSSiCrNiCuFe
0.1510.0150.514-1772 min0.56.0-10.0
Inconel 601(UNS NO6601)(Max.)
CMNSiCrNiCOAIFe
0.050.30.222.561.5min51.414.1
Inconel 718(UNS NO7718)(Max.)
CrNiMoCOCb+TaTiAIFe
1952.5min3.0555.130.90.518.5
Chemical Analysis of Incoloy 800® uns(N08800)
CCrNiTiAIFeGrain
0.1 max19.0-23.030.0-35.00.15-0.60.15-0.639.5min/
Incoloy800H® UNS(N08810)
CCrNiTiAIFeGrain
0.05-0.119.0-23.030.0-35.00.15-0.600.15-0.6039.5min5or coarser
Incoloy800HT® UNS(N08811)
CCrNiTiAIFeGrain
0.06-0.1019.0-23.030.0-35.00.25-0.600.25-0.6039.5min5or coarser

Dimensions:as per drawings


Production Process

Step 1: Getting orders.


Step 2: Process design by technical department


Step 3: Purchase of raw materials and pattern making &checking


Step 4: Inspection of raw materials


Step 5: Melting by middle-frequency induction furnaces


Step 6: Ladle analysis by Spectrometer


Step 7: De-oxidization, slag-removal, tapping


Step 8: Pouring


Step 9: Openning & fettling


Step 10: Surface & dimensional check


Step 11: Heat treatment


Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)


Step 13: Packing


Step 14: Shipping


1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.



Our Trade Show


Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.


Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

www.ebcastings.com


Eternal Bliss Alloy Casting & Forging Co.,LTD.
Quality Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products for sale
Send your message to this supplier
 
*From:
*To: Eternal Bliss Alloy Casting & Forging Co.,LTD.
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0