ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy Wire

Categories Inconel Alloy
Brand Name: KAIXIN
Model Number: KX-Alloy IN P718
Certification: ISO9001:2015
Place of Origin: China
MOQ: 200KG
Price: To negotiate
Payment Terms: T/T, L/C
Supply Ability: 50~80 TONS per MONTH
Delivery Time: 45~60days
Packaging Details: Wooden Box, size as per guests' request
Shape: Wire,Strip,Rod,Pipe,Plate
Alloy Type: Nickel-based Superalloy
Raw Materials: NI Rem,CR18%,Co9% ,MO2.75%
Executive standard: ASTM
Delivery State: Soft State
Application: Used for disc, brake, fastener, blade and etc
Features: High temperature resistance
Size: Negotiable
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy Wire

KX Inconel 718 Plus Nickel Alloy Wire Round Bar Tube Steel Sheet Light Rod On Inconel Alloy


Product Description and Application

Inconel718 plus is a new type of nickel-based precipitation-hardened alloy, which is widely concerned at home and abroad because of its excellent comprehensive mechanical properties below 700°C, good thermal working and welding properties, suitable cost. At present, this material has been promoted and applied in several well-known aero-engine companies, which are used in disc parts, brakes, fasteners, blades and etc. In addition, Inconel718 Plus is also commonly used in copper extrusion mold.


Process Performance and Requirements


  • Product Fusion Process

Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)


  • Product Chemical Composition

ElementCNiCrMoWCoFeNbTiAlPB
Inconel718 plus0.02Rem182.7519105.450.71.450.010.004

  • Product Physical Property

Density8.25g/cm3
Melting Temperature Range1260~1340℃

  • Product Mechanical Property

Hardness:

The hardness is about 20-30HRC after solid solution heat treatment and about 38-45HRC after annealing


  • Productive Process


  • Professional Customization

Cold-drawn Wire¢0.3~¢18mm(Delivery in rolls or trays)
Hot-Rolling Wire¢5.5~¢20mm(Delivery in rolls)
Stripthickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips)
Smooth Forged Rod on a Lathe

¢60~350mm,L800-2500mm

Hot-rolled Burnishing¢20~80mm,L1000-5000mm
Cold Drawn and Burnishing¢2.5~18mm,L1000-8000mm
Seamless Tube¢1~275mm,wall thickness 0.2~30,L1000-8000mm

Quality ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy Wire for sale
Send your message to this supplier
 
*From:
*To: Danyang Kaixin Alloy Material Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0