| Sign In | Join Free | My futurenowinc.com |
|
| Categories | Low Expansion Alloy |
|---|---|
| Brand Name: | HUONA |
| Model Number: | AuNi5 |
| Certification: | ISO9001 |
| Place of Origin: | CHINA |
| MOQ: | 10 g |
| Price: | Bargain |
| Payment Terms: | L/C,T/T,Western Union,MoneyGram |
| Supply Ability: | 1 Ton/Month |
| Delivery Time: | 5-21days |
| Packaging Details: | Carton |
| Resistivity: | 0.14 |
| Specification: | 0.02-0.5mm |
| Product Type: | Wire |
| Material: | Auni5 |
| HS Code: | 7505220000 |
| Product Name: | Gold Nickel Wire |
| Company Info. |
| Huona (Shanghai) New Material Co., Ltd. |
| Verified Supplier |
| View Contact Details |
| Product List |
1,Factory supply with best price
2,Diameter: from0.03mm-0.5mm
3,Used in nonstandard thermocouple
4, TCR: 0.00071
5,Thermal EMF Vs Copper(µv/C) : -0.5
6, T.S. Annealed: 490MPa
Description.
The alloy has been used in "nonstandard" thermocouples, electrical contacts and for electrodes in medical research. The alloy is harder and mechanically stronger than Platinum.
This wire features a 90% Platinum and 10% Iridium composition and is widely used in the assembly of microelectrode probes. Iridium, a Platinum group metal, is very dense and hard, imparting added strength to the wire.
PtIr 5,PtIr10,PtIr15,PtIr20,PtIr25 resistivity: 0.19-0.33 µOhm.m
Technical Data for Platinum/Iridium wire
Electrical Properties
Electrical resistivity ( µOhm.m ): 0.245
Temperature coefficient ( K-1 ): 0.0013
Mechanical Properties
Elongation at break ( % ) <25
Hardness - Brinell 130-190
Tensile strength ( MPa )380-620
Physical Properties
Density ( g cm-3 )21.56
Melting point ( C )1800
Thermal Properties
Coefficient of thermal expansion @20-100C ( x10-6 K-1 )8.7
Thermal conductivity @23C ( W m-1 K-1 )31
Typical Analysis : (ppm)
Ag 100, Au 75, Cu 50, Fe 250, Ir 10%, Ni <100, Si <50, Pt. balance.
Tolerances
Wire diameter: ±10%