| Sign In | Join Free | My futurenowinc.com |
|
| Categories | Nickel Alloy Rod |
|---|---|
| Brand Name: | Zhonggong Special Metallurgy |
| Model Number: | GH4145 alloy |
| Place of Origin: | China |
| MOQ: | 100KG |
| Price: | Price is negotiated based on the required specifications and quantity |
| Payment Terms: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
| Supply Ability: | 5000 tons per month |
| Delivery Time: | 5-8 working days, depending on the parameters required for negotiation |
| Packaging Details: | Standard export packaging, or packaging as required |
| Density: | ~8.3 g/cm³ |
| Melting Point: | ~1390°C (2530°F) |
| Thermal Conductivity: | ~11-12 W/m·K |
| Yield Strength: | ~700 MPa (102 ksi) |
| ~700 MPa (102 ksi): | 900 MPa (130 ksi) |
| Elongation: | ~10% |
| Hardness (Rockwell): | ~HRB 90-95 |
| Applications: | Aerospace components, gas turbines, and high-temperature industrial parts |
| Certification: | ISO Certificate |
GH4145 Alloy
GH4145 is a high-performance nickel-based superalloy renowned for its exceptional strength, thermal stability, and resistance to oxidation and corrosion. It is designed for use in demanding high-temperature environments where reliability and durability are critical.
Key Features:
GH4145 alloy’s superior combination of strength, thermal resistance, and corrosion protection makes it an ideal material for critical applications that require reliable performance in challenging conditions.
Here’s a detailed composition table for GH4145 alloy:
| Element | Content Range |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 18.0-21.0% |
| Iron (Fe) | 14.0-17.0% |
| Cobalt (Co) | 8.0-10.0% |
| Molybdenum (Mo) | 2.0-3.0% |
| Titanium (Ti) | 1.5-2.5% |
| Aluminum (Al) | 1.0-1.5% |
| Boron (B) | 0.005-0.015% |
This table provides a clear overview of the chemical composition of GH4145 alloy, detailing the content ranges of its key elements.

|